Modelling the creep anisotropy of nickel-base superalloys with a composite model
L. Müller

Modelling the creep anisotropy of nickel-base superalloys with a composite model

Author / Organization:
Science & Mathematics Published 1993 Verification Pending

Overview & Synopsis

The creep anisotropy of nickel-base superalloys with a cubic γ' morphology is studied with a composite model. Creep curves and the internal stress distribution in the microstructure under [011] load are calculated with a Finite Element Procedure. Analytical considerations are made for arbitrary loading directions. γ' cubes (with their interfaces aligned parallel to {001} planes) under [001] load have a significant larger creep strength than under [011] or [111] load. Under [011] load the matrix deformation is mainly concentrated in the roof matrix channels.

Advertisement
SPONSOR CONTENT
Indexed from repository: HAL Open Science (hal.science)
Loading document from verified source...
Keyboard Shortcuts: ← / → for pages • + / - for zoom • 0 to fit width Powered by Mozilla PDF.js v3.11

Document Information

Document Title Modelling the creep anisotropy of nickel-base superalloys with a composite model
Author / Organization L. Müller
Subject & Discipline Multidisciplinary Academic Open Research
Categories Science & Mathematics
Publication Year 1993
License / Rights Open Access / Creative Commons
Resource Verification Listed PDF (Verification Pending)
Original Host Website HAL Open Science (hal.science)
File Format application/pdf (Portable Document Format)
Language EN
Catalog ID DOC-80433
Original Source Link Visit Source Page on hal.science »