Nanoskalige Analytik der Mikrostruktur von hochdosig bestrahltem Beryllium
Zimber, Nikolai

Nanoskalige Analytik der Mikrostruktur von hochdosig bestrahltem Beryllium

Author / Organization:
Open Access Books Published 2022 Verification Pending

Overview & Synopsis

The aim of the present work is to develop an in-depth understanding of the microstructural changes in neutron-irradiated beryllium. In particular, it aims to reveal the precise mechanisms leading to the observed tritium retention.Both, helium and tritium could be detected for the first time by high-resolution electron energy loss spectroscopy (EELS) within bubbles in the grain interior as well as along grain boundaries.

Advertisement
SPONSOR CONTENT
Indexed from repository: Directory of Open Access Books (www.doabooks.org)
Loading document from verified source...
Keyboard Shortcuts: ← / → for pages • + / - for zoom • 0 to fit width Powered by Mozilla PDF.js v3.11

Document Information

Document Title Nanoskalige Analytik der Mikrostruktur von hochdosig bestrahltem Beryllium
Author / Organization Zimber, Nikolai
Subject & Discipline Beryllium
Categories Open Access Books
Publication Year 2022
License / Rights Open Access / Creative Commons
Resource Verification Listed PDF (Verification Pending)
Original Host Website Directory of Open Access Books (www.doabooks.org)
File Format application/pdf (Portable Document Format)
Language EN
Catalog ID DOC-32579
Original Source Link Visit Source Page on www.doabooks.org »