CORRELATION BETWEEN AGEING HEAT TREATMENTS, MICROSTRUCTURE AND STRESS CORROSION PROPERTIES OF Al-Li-Cu-Mg ALLOYS
Mumtaz Ahmad

CORRELATION BETWEEN AGEING HEAT TREATMENTS, MICROSTRUCTURE AND STRESS CORROSION PROPERTIES OF Al-Li-Cu-Mg ALLOYS

Author / Organization:
Science & Mathematics Published 1987 Verification Pending

Overview & Synopsis

Stress corrosion cracking (SCC) behaviour of 8090 alloy (Al-Li-Cu-Mg) has been studied using precracked double cantilever beam (DCB) specimens and tuning fork type smooth test specimens. The alloy was SCC tested in several ageing conditions. Although stress corrosion cracks readily initiate when the alloy is exposed to 3.5 % NaCl environment, crack growth is difficult. The SCC performance of the 8090 alloy has been compared with that of 7075-T651 alloy. Fracture toughness of the alloy in a variety of ageing heat treatment conditions was determined by using chevron-notched short bar specimens. Ageing response of the alloy has been determined by hardness measurements and electrical conductivity measurernents.

Indexed from repository: HAL Open Science (hal.science)
Loading document from verified source...
Keyboard Shortcuts: ← / → for pages • + / - for zoom • 0 to fit width Powered by Mozilla PDF.js v3.11

Document Information

Document Title CORRELATION BETWEEN AGEING HEAT TREATMENTS, MICROSTRUCTURE AND STRESS CORROSION PROPERTIES OF Al-Li-Cu-Mg ALLOYS
Author / Organization Mumtaz Ahmad
Subject & Discipline Multidisciplinary Academic Open Research
Categories Science & Mathematics
Publication Year 1987
License / Rights Open Access / Creative Commons
Resource Verification Listed PDF (Verification Pending)
Original Host Website HAL Open Science (hal.science)
File Format application/pdf (Portable Document Format)
Language EN
Catalog ID DOC-247296
Original Source Link Visit Source Page on hal.science »